Vacuum metallizing evaporates aluminum in a vacuum chamber so it condenses onto PET film as a layer only hundreds of angstroms thick. Optical density (OD) is −log10 of transmittance: OD 2.0 passes at most about 1% of light. Expansteel specifies aluminum OD ≥ 2.0 on ES-VM and ES-VM Plus, ≥ 1.5 on ES-H and ≥ 2.5 on ES-H03.
Aluminum is evaporated inside a vacuum chamber and condenses onto a moving polyester (PET) carrier film as a continuous metal layer, typically hundreds of angstroms thick. The aluminum bonds into the film surface, producing a dense reflective layer rather than a coated-on surface treatment. Because the layer reflects light instead of absorbing it, one deposition pass can do the blackout or reflective work that would otherwise take several pigment coating passes.
Expansteel runs vacuum metallizing and non-woven lamination in-house, on 12 μm standard PET (customizable from 6 to 100 μm), in widths up to 2400 mm.
Optical density is logarithmic: OD = −log10(T), so transmittance T = 10−OD. The table gives the theoretical maximum light passing through the metal layer alone at each OD.
| Optical density (OD) | Max. light transmittance (calculated) |
|---|---|
| 1.0 | 10% |
| 1.5 | ≈ 3.2% |
| 2.0 | 1% |
| 2.5 | ≈ 0.32% |
| 3.0 | 0.1% |
Values are calculated from the formula, not separate lab results. Because OD is logarithmic, small OD increases are large increases in blocking. The ES-VM Plus TDS specifies the finished film at ≈ 0% light transmittance.
Expansteel recommends choosing the grade by application, not by OD alone: ES-VM Plus for total-blackout shade cores, ES-VM for general metallized layers and insulation, and the ES-H series where gas barrier is the job.
| Grade | Aluminum OD | Other published figures | Typical use |
|---|---|---|---|
| ES-VM | ≥ 2.0 (typical 2.0) | Al adhesion 1.5 N/15mm; 6–100 μm customizable | General-purpose metallized layer, semi-blackout grades, insulation, decoration |
| ES-VM Plus | ≥ 2.0 (typical 2.0) | Light transmittance ≈ 0%; UV-aging Pass | Total-blackout core for cellular, pleated and roller shades |
| ES-H | ≥ 1.5 | OTR ≤ 1.0 cc/m²·24h | Entry-tier high barrier: coffee, oxidation-sensitive snacks |
| ES-H03 | ≥ 2.5 | OTR ≤ 0.1 cc/m²·24h; WVTR ≤ 0.3 g/m²·24h | Ultra-high barrier and full light block |
Vacuum metallizing is a physical vapor deposition process: aluminum is evaporated inside a vacuum chamber and condenses onto a moving PET film as a continuous layer only hundreds of angstroms thick. The metal bonds into the film surface instead of being a separate sheet, which is why metallized film behaves differently from aluminum foil.
OD is a logarithmic measure of light blocking: OD = −log10(transmittance). OD 1.0 passes at most 10% of light, OD 2.0 at most 1% and OD 3.0 at most 0.1%. On the Expansteel ES-VM and ES-VM Plus data sheets the aluminum layer is reported in O.D. units with the test method GB/T15717 listed.
Expansteel specifies aluminum OD ≥ 2.0 for ES-VM Plus, the blackout-grade film, and the finished film is specified at a light transmittance of ≈ 0%. The OD table on this page is calculated for the metal layer alone; the ≈ 0% figure is the finished film's TDS specification.
No. Match the grade to the requirement: barrier performance also depends on coating integrity and adhesion, not on OD alone, so choose by the application's oxygen, moisture and light requirements.
Yes. For window-film base film Expansteel deposits to a customer-specified optical density — from a thick blackout layer (OD ≥ 2.0) to an ultra-thin translucent layer that reflects infrared while passing visible light.
Each ES grade's data sheet lists the aluminum layer's optical density, and a Certificate of Analysis (COA) accompanies every shipment. Download the data sheets from the TDS page or request a sample.
Every inquiry and sample request is reviewed by our technical team — lead times and sample logistics are confirmed in the first reply, within one business day.
Request a Sample →